Nanoindentation and Atomic Force Microscopy Measurements on Reactively Sputtered Tin Coatings
Total Page:16
File Type:pdf, Size:1020Kb
Load more
Recommended publications
-
Nanoindentations in Kinking Nonlinear Elastic Solids
Nanoindentations in Kinking Nonlinear Elastic Solids A Thesis Submitted to the Faculty of Drexel University by Anand Murugaiah in partial fulfillment of the requirements for the degree of Doctor of Philosophy May 2004 ii ACKNOWLEDGMENTS I am very grateful to a lot of people who were instrumental in my studies at Drexel University. First, I would like to thank my advisors, Dr. Michel W. Barsoum and Dr. Surya Kalidindi for their help, guidance, support and patience during trying times. I have learnt so much under their tutelage. They have been there always to correct me, guide me, motivate me and work with me. I am truly fortunate to have them as my advisors. I am grateful to Dr. Tamer El-Raghy for his help and guidance during my research. I am very thankful to my thesis committee: Prof. Yury Gogotsi, Dr. David Stepp (Army Research Labs) and Dr. El-Raghy for their time, help and assistance in helping me complete my work. I also would like to thank the Department of Materials Science and Engineering, the faculty, staff and my dear colleagues for their support and those wonderful moments that I shared with them. I would like to thank my family and friends for being there for me when I needed them. I would like to thank Prof. Y. Gogotsi again for many stimulating and useful discussions and Mr. Thomas F. Juliano, for his help with the nanoindenter. I am also grateful to Dr. T. El-Raghy of 3-ONE-2 LLC for supplying the Ti3SiC2 samples. The graphite single crystals were provided by Prof. -
Novel Nanoindentation-Based Techniques for MEMS and Microfluidics Applications Ke Du University of South Florida
University of South Florida Scholar Commons Graduate Theses and Dissertations Graduate School 11-7-2008 Novel Nanoindentation-Based Techniques for MEMS and Microfluidics Applications Ke Du University of South Florida Follow this and additional works at: https://scholarcommons.usf.edu/etd Part of the American Studies Commons Scholar Commons Citation Du, Ke, "Novel Nanoindentation-Based Techniques for MEMS and Microfluidics Applications" (2008). Graduate Theses and Dissertations. https://scholarcommons.usf.edu/etd/220 This Thesis is brought to you for free and open access by the Graduate School at Scholar Commons. It has been accepted for inclusion in Graduate Theses and Dissertations by an authorized administrator of Scholar Commons. For more information, please contact scholarcommons@usf.edu. Novel Nanoindentation-Based Techniques for MEMS and Microfluidics Applications by Ke Du A thesis submitted in partial fulfillment of the requirements for the degree of Master of Science in Mechanical Engineering Department of Mechanical Engineering College of Engineering University of South Florida Major Professor: Alex. A. Volinsky, Ph.D. Craig Lusk, Ph.D. Nathan Crane, Ph.D. Date of Approval: November 7, 2008 Keywords: thin films, mechanical properties, compliant MEMS, electrowetting © Copyright 2008 , Ke Du Dedication I would like to dedicate this manuscript to my relatives, especially my parents. Thanks for their support and encouragement throughout the years. Acknowledgements I would like to thank for my advisor Dr. Volinsky. Without his guidance, -
Nanotechnology for the Forest Products Industry Vision and Technology Roadmap
Nanotechnology for the Forest Products Industry—Vision and Technology Roadmap iii Table of Contents Executive Summary .......................................................................................................... v 1—Overview of the Forest Products Industry ................................................................... 1 2—Vision for Nanotechnology in the Forest Products Industry ....................................... 7 3—R&D Strategy ............................................................................................................ 11 R&D Focus Area 1 Polymer Composites and Nano-Reinforced Materials .............................................. 17 R&D Focus Area 2 Self-Assembly and Biomimetics ................................................................................ 23 R&D Focus Area 3 Cell Wall Nanotechnology ....................................................................................... 27 R&D Focus Area 4 Nanotechnology in Sensors, Processing, and Process Control ................................. 33 R&D Focus Area 5 Analytical Methods for Nanostructure Characterization ......................................... 37 R&D Focus Area 6 Collaboration in Advancing Programs and Conducting Research ........................... 43 4—Implementation Plan: Next Steps and Recommendations ........................................ 45 Appendices .................................................................................................................... 49 A—Workshop Agenda........................................................................................ -
Pencil Hardness
Measuring Coating Mechanical Properties CTT 2019 Rahul Nair Fischer Technology, Inc. 2018 1 Coating Mechanical Properties Characterization Nanoindentation Progressive Load Scratch Fischer Technology, Inc. 2018 2 Characterizing Surfaces Treated surfaces Coatings and Thin Films Composites Fischer Technology, Inc. 2018 3 Coating Mechanical Properties Characterization Fischer Technology, Inc. 2018 4 Coating Mechanical Properties Characterization H a r d n e s s I C r e e p I E l a s t i c i t y I U n i a x i a l M e c h a n i c a l R e s p o n s e I Te n s i l e S t r e n g t h and Te n s i l e S t r e s s I S t i f f n e s s in Te n s i o n - Yo u n g ’ s M o d u l u s I T h e P o i s s o n E f f e c t I S h e a r i n g S t r e s s e s and S t r a i n s S t r e s s - S t r a i n C u r v e s Thermodynamics of M e c h a n i c a l R e s p o n s e I E n t h a l p i c R e s p o n s e I E n t r o p i c R e s p o n s e I Viscoelasticity I S t i f f n e s s I K i n e m a t i c s : the S t r a i n – Displacement R e l a t i o n s I Equilibrium : the S t r e s s R e l a t i o n s I Transformation of S t r e s s e s and S t r a i n s Constitutive I Y i e l d and P l a s t i c F l o w I M u l t i a x i a l S t r e s s S t a t e s I E f f e c t of Hydrostatic P r e s s u r e I E f f e c t of Rate and Temperature I C o n t i n u u m P l a s t i c i t y I T h e Dislocation B a s i s of Y i e l d and C r e e p K i n e t i c s of C r e e p in Crystalline M a t e r i a l s I F r a c t u r e I A t o m i s t i c s of C r e e p R u p t u r e I F r a c t u r e M e c h a n i c s - the E n e r g y - B a l a n c e A p p r o a c h I the S t r e s s I n t e n s i t y A p p r o a c h I F a t i g u e Fischer Technology, Inc. -
Experimental Correlation of Mechanical Properties of the Ti-6Al-4V Alloy at Different Length Scales
metals Article Experimental Correlation of Mechanical Properties of the Ti-6Al-4V Alloy at Different Length Scales Víctor Tuninetti 1,* , Andrés Felipe Jaramillo 1 , Guiomar Riu 2, Carlos Rojas-Ulloa 1 , Amna Znaidi 3, Carlos Medina 4 , Antonio Manuel Mateo 2 and Joan Josep Roa 2,* 1 Department of Mechanical Engineering, Universidad de La Frontera, 4780000 Temuco, Chile; andresfelipe.jaramillo@ufrontera.cl (A.F.J.); c.rojas13@ufromail.cl (C.R.-U.) 2 Department of Materials Science and Engineering (CIEFMA), Barcelona School of Engineering (EEBE), Universitat Politècnica de Catalunya-BarcelonaTech, 08019 Barcelona, Spain; guiomarriu@gmail.com (G.R.); antonio.manuel.mateo@upc.edu (A.M.M.) 3 Laboratory of Applied Mechanics and Engineering LR-MAI, University Tunis El Manar–ENIT BP37, Tunis 1068, Tunisia; amna.znaidi@ipeiem.utm.tn 4 Department of Mechanical Engineering, Universidad de Concepción, 4030000 Concepción, Chile; cmedinam@udec.cl * Correspondence: victor.tuninetti@ufrontera.cl (V.T.); joan.josep.roa@upc.edu (J.J.R.); Tel.: +56-452325984 (V.T.); +34-93-413-41-39 (J.J.R.) Abstract: This article focuses on a systematic study of a Ti-6Al-4V alloy in order to extensively characterize the main mechanical properties at the macro-, micro- and submicrometric length scale under different stress fields. Hardness, elastic modulus, true stress–strain curves and strain-hardening exponent are correlated with the intrinsic properties of the a- and b-phases that constitute this alloy. A systematic characterization process followed, considering the -
Cobalt Composites As a Function of Tungsten Carbide Crystal Orientation
Article Nano-Indentation Properties of Tungsten Carbide- Cobalt Composites as a Function of Tungsten Carbide Crystal Orientation Renato Pero 1, Giovanni Maizza 2,*, Roberto Montanari 1 and Takahito Ohmura 3 1 Department of Industrial Engineering, University of Rome “Tor Vergata”, 00133 Rome, Italy; renato.pero@alumni.uniroma2.eu (R.P.); roberto.montanari@uniroma2.it (R.M.) 2 Department of Applied Science and Technology, Politecnico di Torino, 10129 Torino, Italy 3 High Strength Materials Group, National Institute for Materials Science (NIMS), 1-2-1 Sengen, Ibaraki Tsukuba 305-0047, Japan; ohmura.takahito@nims.go.jp * Corresponding author: giovanni.maizza@polito.it Received: 4 April 2020; Accepted: 28 April 2020; Published: 5 May 2020 Abstract: Tungsten carbide-cobalt (WC-Co) composites are a class of advanced materials that have unique properties, such as wear resistance, hardness, strength, fracture-toughness and both high temperature and chemical stability. It is well known that the local indentation properties (i.e., nano- and micro-hardness) of the single crystal WC particles dispersed in such composite materials are highly anisotropic. In this paper, the nanoindentation response of the WC grains of a compact, full- density, sintered WC-10Co composite material has been investigated as a function of the crystal orientation. Our nanoindentation survey has shown that the nanohardness was distributed according to a bimodal function. This function was post-processed using the unique features of the finite mixture modelling theory. The combination of electron backscattered diffraction (EBSD) and statistical analysis has made it possible to identify the orientation of the WC crystal and the distinct association of the inherent nanoindentation properties, even for a small set (67) of nanoindentations. -
Operando Nanoindentation
A3840 Journal of The Electrochemical Society, 164 (14) A3840-A3847 (2017) Operando Nanoindentation: A New Platform to Measure the Mechanical Properties of Electrodes during Electrochemical Reactions Luize Scalco de Vasconcelos, Rong Xu, and Kejie Zhao∗,z School of Mechanical Engineering, Purdue University, West Lafayette, Indiana 47907, USA We present an experimental platform of operando nanoindentation that probes the dynamic mechanical behaviors of electrodes during real-time electrochemical reactions. The setup consists of a nanoindenter, an electrochemical station, and a custom fluid cell integrated into an inert environment. We evaluate the influence of the argon atmosphere, electrolyte solution, structural degradation and volumetric change of electrodes upon Li reactions, as well as the surface layer and substrate effects by control experiments. Results inform on the system limitations and capabilities, and provide guidelines on the best experimental practices. Furthermore, we present a thorough investigation of the elastic-viscoplastic properties of amorphous Si electrodes, during cell operation at different C-rates and at open circuit. Pure Li metal is characterized separately. We measure the continuous evolution of the elastic modulus, hardness, and creep stress exponent of lithiated Si and compare the results with prior reports. operando indentation will provide a reliable platform to understand the fundamental coupling between mechanics and electrochemistry in energy materials. © The Author(s) 2017. Published by ECS. This is an open access article distributed under the terms of the Creative Commons Attribution 4.0 License (CC BY, http://creativecommons.org/licenses/by/4.0/), which permits unrestricted reuse of the work in any medium, provided the original work is properly cited. -
Indentation Hardness Measurements at Macro-, Micro-, and Nanoscale: a Critical Overview
Tribol Lett (2017) 65:23 DOI 10.1007/s11249-016-0805-5 REVIEW Indentation Hardness Measurements at Macro-, Micro-, and Nanoscale: A Critical Overview Esteban Broitman1 Received: 25 September 2016 / Accepted: 15 December 2016 / Published online: 28 December 2016 Ó The Author(s) 2016. This article is published with open access at Springerlink.com Abstract The Brinell, Vickers, Meyer, Rockwell, Shore, 1 Introduction IHRD, Knoop, Buchholz, and nanoindentation methods used to measure the indentation hardness of materials at The hardness of a solid material can be defined as a mea- different scales are compared, and main issues and mis- sure of its resistance to a permanent shape change when a conceptions in the understanding of these methods are constant compressive force is applied. The deformation can comprehensively reviewed and discussed. Basic equations be produced by different mechanisms, like indentation, and parameters employed to calculate hardness are clearly scratching, cutting, mechanical wear, or bending. In metals, explained, and the different international standards for each ceramics, and most of polymers, the hardness is related to method are summarized. The limits for each scale are the plastic deformation of the surface. Hardness has also a explored, and the different forms to calculate hardness in close relation to other mechanical properties like strength, each method are compared and established. The influence ductility, and fatigue resistance, and therefore, hardness of elasticity and plasticity of the material in each mea- testing can be used in the industry as a simple, fast, and surement method is reviewed, and the impact of the surface relatively cheap material quality control method. -
Nanoindentation Technique for Characterizing Cantilever Beam Style RF Microelectromechanical Systems (MEMS) Switches Hyukjae Lee Air Force Institute of Technology
Marquette University e-Publications@Marquette Electrical and Computer Engineering Faculty Electrical and Computer Engineering, Department Research and Publications of 4-29-2005 Nanoindentation Technique for Characterizing Cantilever Beam Style RF Microelectromechanical Systems (MEMS) Switches Hyukjae Lee Air Force Institute of Technology Ronald A. Coutu Jr. Marquette University, ronald.coutu@marquette.edu Shankar Mall Air Force Institute of Technology Paul E. Kladitis Air Force Institute of Technology Accepted version. Journal of Micromechanics and Microengineering, Vol. 15, No. 6 (April 29, 2006): 1230. DOI. © 2006 IOP Publishing. Used with permission. Ronald A Coutu Jr. Sensors Directorate, Air Force Research Laboratory, Wright-Patterson Air Force Base, OH at the time of publication. Marquette University e-Publications@Marquette Electrical and Computer Engineering Faculty Research and Publications/College of Engineering This paper is NOT THE PUBLISHED VERSION; but the author’s final, peer-reviewed manuscript. The published version may be accessed by following the link in the citation below. Journal of Micromechanics and Microengineering, Vol. 15, No. 6, (April, 2005): 1230-1235. DOI. This article is © Institute of Physics and permission has been granted for this version to appear in e-Publications@Marquette. Institute of Physics does not grant permission for this article to be further copied/distributed or hosted elsewhere without the express permission from Institute of Physics. Contents Abstract ........................................................................................................................................................ -
Nanoindentation and XPS Studies of Titanium TNZ Alloy After Electrochemical Polishing in a Magnetic Field
Materials 2015, 8, 205-215; doi:10.3390/ma8010205 OPEN ACCESS materials ISSN 1996-1944 www.mdpi.com/journal/materials Article Nanoindentation and XPS Studies of Titanium TNZ Alloy after Electrochemical Polishing in a Magnetic Field Tadeusz Hryniewicz 1,†,*, Krzysztof Rokosz 1,†, Ryszard Rokicki 2 and Frédéric Prima 3 1 Division of Surface Electrochemistry, Koszalin University of Technology, Racławicka 15-17, Koszalin 75-620, Poland; E-Mail: rokosz@tu.koszalin.pl 2 Electrobright, 142 W. Main St., Macungie, PA 18062, USA; E-Mail: ryszardr@ptd.net 3 Institut de Recherche de Chimie Paris, CNRS–Chimie ParisTech, 11 rue Pierre et Marie Curie, Paris 75005, France; E-Mail: frederic.prima@chimie-paristech.fr † These authors contributed equally to this work. * Author to whom correspondence should be addressed; E-Mail: Tadeusz.Hryniewicz@tu.koszalin.pl; Tel.: +48-94-3478244. Academic Editor: Daolun Chen Received: 19 September 2014 / Accepted: 25 December 2014 / Published: 8 January 2015 Abstract: This work presents the nanoindentation and XPS results of a newly-developed biomaterial of titanium TNZ alloy after different surface treatments. The investigations were performed on the samples AR (as received), EP (after a standard electropolishing) and MEP (after magnetoelectropolishing). The electropolishing processes, both EP and MEP, were conducted in the same proprietary electrolyte based on concentrated sulfuric acid. The mechanical properties of the titanium TNZ alloy biomaterial demonstrated an evident dependence on the surface treatment method, with MEP samples revealing extremely different behavior and mechanical properties. The reason for that different behavior appeared to be influenced by the surface film composition, as revealed by XPS study results displayed in this work. -
The Edge Effect in Nanoindentation Joseph E
Philosophical Magazine 2010, 1-13, iFirst The edge effect in nanoindentation Joseph E. Jakesab and Donald S. Stoneac* aMaterials Science Program, University of Wisconsin-Madison, Madison, Wisconsin, USA; bPerformance Enhanced Biopolymers, United States Forest Service, Forest Products Laboratory, Madison, Wisconsin, USA; ‘Department of Materials Science and Engineering, University of Wisconsin-Madison, Madison, Wisconsin, USA (Received 23 October 2009; final version received 19 May 2010) Until recently, obtaining unambiguous data from a nanoindentation measurement placed near a free edge has not been possible because the discontinuity associated with the edge introduces artifacts into the measurement. The primary consequence of a free edge is to introduce a structural compliance, Cs, into the measurement. Like the machine compliance, Cm, Cs is independent of the size of the indent and it adds to the measured unloading compliance; but unlike Cm, Cs is a function of position. Accounting for Cs in nanoindentation analyses removes the artifacts in nanoindentation measurements associated with the edge, allowing researchers to more accurately probe material properties near an edge. Expressions were obtained for the effect of the free edge on hardness and modulus measured using the Oliver-Pharr method. The theory was tested on specimens including fused silica, poly(methyl methacrylate), and alayered silicon-on-insulatorspecimen. Keywords: nanoindentation; edge effect 1. Introduction A key capability of nanoindentation is its ability to probe local mechanical properties in specimens that are highly non-uniform. Determining how properties change near an edge, such as the interface between phases or a free edge, is often of interest. The problem with making those kinds of measurements is that, above and beyond any effect associated with changes in properties near the edge, the presence of the elastic discontinuity will itself give rise to effects, i.e. -
Nanotechnology Applications in the Forest Products Industry by Robert J
Nanotechnology Applications in the Forest Products Industry By Robert J. Moon, Charles R. Frihart, and Theodore Wegner The National Nanotechnology Initiative (NNI) was has grown to 12 and 25, respectively.1 The vision of the NNI established in 2001 to coordinate the R&D of nanoscale sci is a future in which the ability to understand and control ence, engineering, and technology across the federal gov matter at the nanoscale level leads to a revolution in tech ernment. The Nanoscale Science, Engineering and nology and industry. The four goals of NNI are to 1) maintain Technology Subcommittee coordinates in the NNI and oper a world-class R&D program aimed at realizing the full poten ates under the auspices of the National Science and tial of nanotechnology; 2) facilitate transfer of new tech Technology Council. In its first year, NNI was composed of nologies into products for economic growth, jobs, and other six agencies investing in nanotechnology. Since that time, public benefits; 3) support responsible development of nan the annual federal investment has more than doubled in otechnology; and 4) develop educational resources, a nanotechnology R&D to approximately $1.3 billion, while skilled workforce, and the supporting infrastructure and the number of funding and participating federal agencies tools to advance nanotechnology. In addition, the NNI is 4 MAY 2006 developing a national infrastructure that will provide access products industry to include paper, composites, and solid to user centers that house expensive and sophisticated sawnlumber.Specifically,thealliancehasidentifiedsixmajor equipment that is necessary but not cost effective for any areas of technological needs: 1) advancing the forest biorefin one group or institution to purchase and maintain.