Surface Analysis of Nuclear Graphite

Total Page:16

File Type:pdf, Size:1020Kb

Load more

Keywords Surface analysis Graphite, XPS, 2 of nuclear graphite Auger d-parameter, sp Application Note MO426(1) Further application/technical notes are available online at: www.kratos.com Overview Introduction In this short study we will explore the differences in Graphite is one of the key materials used in the current generation of nuclear reactors in the UK. Since the early days of nuclear fission surface chemistry between two different graphites used graphite has been recognised as an excellent neutron moderator in the nuclear industry. In recent times a wide variety and reflector allowing sustainable controlled fission. of nanostructured carbon forms have been observed in Contaminants in moderator rods are a major problem as they nuclear graphite which vary the graphitic nature of the can act as neutron absorbers. This causes decreased fission and material. The nature of these forms can greatly affect production of unwanted isotopes – a common cause of radioactive waste. The goal of this application is to understand the surface the material’s ability to act as an effective moderator. chemistry of two different graphites: Pile Grade A (PGA) and Here we will discuss the elemental composition of the Gilsocarbon (Gilso). PGA is an early form of nuclear graphite used graphite surface and the extent of graphitic sp2 bonding. in many reactors world-wide, particularly in the UK in the Magnox series. It is derived from a petroleum coke (which is a by-product of the oil refining industry). Gilsocarbon was developed later and is used in the Generation II Advanced Gas-Cooled Reactors. The Gilsonite coke is produced from refining the asphalt. Here we will study the two graphites and try to identify differences in surface chemistry and extent of sp2/sp3 character. Kratos Analytical Ltd. UK APPLICATION NOTES AXIS SERIES Wharfside, Trafford Wharf Road, Manchester M17 1GP Phone: +44 161 888 4400 Fax. +44 161 888 4402 www.kratos.com 400 16.12 eV High resolution C 1s spectra were acquired to identify Experimental Highthe200 resolutionchemical Cstat 1s esspectra of the were carbon acquired in theto identify surface the (figure chemical Figure 3. First derivative C KLL Auger states2). of the carbon in the surface (figure 2). All measurements were acquired using a Kratos Axis Supra XPS. 20.82 eV spectra. The AXIS Supra incorporates several features which make high 0 50 resolution spectroscopic analysis of these types of challenging 230 250 270 290 samples routine: 45 Conclusions -200 40 • A 500 mm Rowland circle Al X-ray monochromator; Two graphite samples were analysed using XPS to 35 dN(E)/ dE • Coaxial charge neutralisation system; determine carbon chemistry at the surface. Small -400 30 concentrations of contaminants were seen on the • Magnetic lens; 25 surface of the Gilsocarbon surface and the high- • 165 mm hemispherical analyser; 20 resolution C 1s spectrum showed less sp2 character -600 • Delay line detector. 15 than for the PGA sample. Further analysis of the Auger parameter allowed the degree of surface sp2:sp3 The two graphitic samples were cut from larger rods using 10 to be quantified. This study highlights the use of the -800 a mechanical saw. 5 AXIS Supra spectrometer in detecting low kinetic energy / eV Results 0 concentration contaminants and in determining 310 300 290 280 bonding arrangements in carbon materials After introducing the graphite samples into the AXIS Supra, survey Binding energy /eV spectra were acquired to identify the elements present on the surface. Figure 1 shows the spectra post automated elemental peak Acknowledgements identification. Figure 2: C 1s spectra for Gilso (green) and PGA (blue). Figure 2: C 1s spectra for Gilso (green) and Many thanks to Dr Alex Theodosiou of the University C 1s PGA (blue). of Manchester for this collaborative study. For both graphite samples the C 1s peak appears at ~284.4 eV. The C 1s spectrum for PGA has an asymmetric line shape towards highFor binding both graphite energy. This samples peak shape the isC typical 1s peak of graphitic appears carbon. at References There~284.4 is also eV. a pronounced The C 1s peak spectrum at >290 eVfor – a shake-upPGA has satellite an 2 [1] T.L. Barr, S. Seal, J. Vac. Sci. Technol. A 13(3) (1995) previouslyasymmetric attributed line shapeto sp bonding. towards In higharomatic binding systems energy. this * 1239. structureThis peak has shapebeen shown is typical to be of due graphitic to π→π carbon.transitions There involving is thealso two a highest pronounced filled orbital peak and at the >290 lowest eV unfilled – a shake orbital.- upIn [2] Scaglione et al. Appl. Surf. Sci., 47 (1991) 17-21. general, the more pronounced the loss peak the2 greater degree Intensity satellite previously attributed to sp bonding. In of sp2 bonding. The Gilso C 1s spectrum differs greatly from PGA. Therearomatic is no longersystems a clearly this structuredefined shake-up has been feature shown and toa shoulder be due to π→π* transitions involving the two highest filled Na 1s O 1s is clear on the high binding energy side of the primary peak ~285- C KLL orbital and the lowest unfilled orbital. In general,3 the O KLL 286 eV. This shoulder is most probably increased sp character and somemore C-O pronounced chemistry. the loss peak the greater degree of sp2 bonding. The Gilso C 1s spectrum differs greatly To gain further information regarding the bonding states of the 1200 1000 800 600 400 200 0 from PGA. There is no longer a clearly defined shake- Binding energy /eV two different graphite samples, carbon KLL Auger electron lines wereup featurealso acquired. and a Following shoulder ionization is clear byon photoelectron the high binding emission Figure 1: Survey spectra for Gilso (green) and PGA (blue). anenergy outer shell side electron of the can primary fill the createdpeak ~285vacancy-286 and eV the. Thisenergy releasedshoulder can is result most in probablythe emission increased of an Auger sp3 electron. character Analysis and Quantification of the survey spectra for the two samples (table 1) ofsome the X-ray C-O inducedchemistry. C KLL Auger peak can help distinguish the showed as expected mainly carbon on the surface with a small bondingTo gain states further in a semi-quantitative information regarding manner for thenon-functionalized bonding amount of surface oxygen. The oxygen can be attributed to a thin samples.states ofScaglione the two et al.different proposed graphite a simple methodsamples, of quantifyingcarbon film of adventitious carbon which is present on all air-exposed the relative amount of sp2/sp3 character in a carbon material KLL Auger electron lines were also acquired. Following samples. Adventitious carbon is generally comprised of short chain, using this first derivitave2. The energy difference between the perhaps polymeric non-graphitic hydrocarbons species with small spectrumionization maximum by photoelectron and minimum isemission known as anthe outerd-parameter shell amounts of both singly and doubly bound oxygen functionality1. andelectron is linearly can related fill the to the created concentration vacancy of spand2 character. the energy Figure No other elements were detected in the PGA surface however 3 releasedshows the firstcan derivativeresult in spectra the foremission the two ofgraphite an Augersamples. several contaminants of low concentration were identified in the Hereelectr thereon. is Analysisa clear distinction of the inX- energyray induced difference C KLLbetween Auger the Gilso sample. peakpeak maximum can help and disti minimumnguish forthe the bonding two graphites. states inPGA a semishows- ~74%quantitative sp2 character manner compared for nonto ~20%-functionalized sp2 character samples.of Gilso. The Element C 0 Si S Na N CI correlationScaglione of resultset al .obtained proposed from thea highsimple resolution method C 1s andof C KLLquantifying spectra indicate the relative that the amountPGA sample’s of sp surface2/sp3 character contains ain higher a PGA 98.70 1.30 - - - - - concentrationcarbon material of graphitic using carbon.this first derivitave2. The energy Gilso 93.92 5.16 0.11 0.07 0.19 0.52 0.03 difference between the spectrum maximum and minimum is known as the d-parameter and is linearly related to the concentration of sp2 character. Figure 3 Table 1: Surface quantification for Gilso and PGA graphite surfaces. shows the first derivative spectra for the two graphite samples. Here there is a clear distinction in energy difference between the peak maximum and minimum for the two graphites. PGA shows ~74% sp2 character compared to ~20% sp2 character of Gilso. The correlation of results obtained from the high resolution C 1s and C KLL spectra indicate that the PGA sample’s surface contains a higher concentration of graphitic carbon. Kratos Analytical Ltd. UK APPLICATION NOTES AXIS SERIES Wharfside, Trafford Wharf Road, Manchester M17 1GP Phone: +44 161 888 4400 Fax. +44 161 888 4402 www.kratos.com TECHNICAL NOTES AXIS SERIES Conclusions 400 16.12 eV Two graphite samples were analysed using XPS to determine carbon chemistry at the surface. Small concentrations of contaminants were seen on the surface of the Gilsocarbon surface and the high- 200 resolution C 1s spectrum showed less sp2 character than for the PGA sample. Further analysis of the Auger parameter allowed the 20.82 eV degree of surface sp2:sp3 to be quantified. This study highlights the 0 use of the AXIS Supra spectrometer in detecting low concentration 230 250 270 290 contaminants and in determining bonding arrangements in carbon materials -200 Acknowledgements Many thanks to Dr Alex Theodosiou of the University of Manchester dN(E)/dE for this collaborative study. -400 References [1] T.L. Barr, S. Seal, J. Vac. Sci. Technol. A 13(3) (1995) 1239. -600 [2] Scaglione et al. Appl. Surf. Sci., 47 (1991) 17-21. -800 kinetic energy /eV Figure 3.
Recommended publications
  • Graphite Materials for the U.S

    Graphite Materials for the U.S

    ANRIC your success is our goal SUBSECTION HH, Subpart A Timothy Burchell CNSC Contract No: 87055-17-0380 R688.1 Technical Seminar on Application of ASME Section III to New Materials for High Temperature Reactors Delivered March 27-28, 2018, Ottawa, Canada TIM BURCHELL BIOGRAPHICAL INFORMATION Dr. Tim Burchell is Distinguished R&D staff member and Team Lead for Nuclear Graphite in the Nuclear Material Science and Technology Group within the Materials Science and Technology Division of the Oak Ridge National Laboratory (ORNL). He is engaged in the development and characterization of carbon and graphite materials for the U.S. Department of Energy. He was the Carbon Materials Technology (CMT) Group Leader and was manager of the Modular High Temperature Gas-Cooled Reactor Graphite Program responsible for the research project to acquire reactor graphite property design data. Currently, Dr. Burchell is the leader of the Next Generation Nuclear Plant graphite development tasks at ORNL. His current research interests include: fracture behavior and modeling of nuclear-grade graphite; the effects of neutron damage on the structure and properties of fission and fusion reactor relevant carbon materials, including isotropic and near isotropic graphite and carbon-carbon composites; radiation creep of graphites, the thermal physical properties of carbon materials. As a Research Officer at Berkeley Nuclear Laboratories in the U.K. he monitored the condition of graphite moderators in gas-cooled power reactors. He is a Battelle Distinguished Inventor; received the Hsun Lee Lecture Award from the Chinese Academy of Science’s Institute of Metals Research in 2006 and the ASTM D02 Committee Eagle your success is our goal Award in 2015.
  • Molten Salt Chemistry Workshop

    Molten Salt Chemistry Workshop

    The cover depicts the chemical and physical complexity of the various species and interfaces within a molten salt reactor. To advance new approaches to molten salt technology development, it is necessary to understand and predict the chemical and physical properties of molten salts under extreme environments; understand their ability to coordinate fissile materials, fertile materials, and fission products; and understand their interfacial reactions with the reactor materials. Modern x-ray and neutron scattering tools and spectroscopy and electrochemical methods can be coupled with advanced computational modeling tools using high performance computing to provide new insights and predictive understanding of the structure, dynamics, and properties of molten salts over a broad range of length and time scales needed for phenomenological understanding. The actual image is a snapshot from an ab initio molecular dynamics simulation of graphene- organic electrolyte interactions. Image courtesy of Bobby G. Sumpter of ORNL. Molten Salt Chemistry Workshop Report for the US Department of Energy, Office of Nuclear Energy Workshop Molten Salt Chemistry Workshop Technology and Applied R&D Needs for Molten Salt Chemistry April 10–12, 2017 Oak Ridge National Laboratory Co-chairs: David F. Williams, Oak Ridge National Laboratory Phillip F. Britt, Oak Ridge National Laboratory Working Group Co-chairs Working Group 1: Physical Chemistry and Salt Properties Alexa Navrotsky, University of California–Davis Mark Williamson, Argonne National Laboratory Working
  • Nuclear Graphite for High Temperature Reactors

    Nuclear Graphite for High Temperature Reactors

    Nuclear Graphite for High temperature Reactors B J Marsden AEA Technology Risley, Warrington Cheshire, WA3 6AT, UK Abstract The cores and reflectors in modem High Temperature Gas Cooled Reactors (HTRs) are constructed from graphite components. There are two main designs; the Pebble Bed design and the Prism design, see Table 1. In both of these designs the graphite not only acts as a moderator, but is also a major structural component that may provide channels for the fuel and coolant gas, channels for control and safety shut off devices and provide thermal and neutron shielding. In addition, graphite components may act as a heat sink or conduction path during reactor trips and transients. During reactor operation, many of the graphite component physical properties are significantly changed by irradiation. These changes lead to the generation of significant internal shrinkage stresses and thermal shut down stresses that could lead to component failure. In addition, if the graphite is irradiated to a very high irradiation dose, irradiation swelling can lead to a rapid reduction in modulus and strength, making the component friable. The irradiation behaviour of graphite is strongly dependent on its virgin microstructure, which is determined by the manufacturing route. Nevertheless, there are available, irradiation data on many obsolete graphites of known microstructures. There is also a well-developed physical understanding of the process of irradiation damage in graphite. This paper proposes a specification for graphite suitable for modem HTRs. HTR Graphite Component Design and Irradiation Environment The details of the HTRs, which have, or are being, been built and operated, are listed in Table 1.
  • Mon. Oct 29, 2018 Room1 Plenary Talk 1

    Mon. Oct 29, 2018 Room1 Plenary Talk 1

    Mon. Oct 29, 2018 Plenary Talk The 9th International Conference on Multiscale Materials Modeling Mon. Oct 29, 2018 Room1 Plenary Talk | Plenary Talk [PL1] Plenary Talk 1 Chair: Ju Li(MIT, USA) 10:10 AM - 11:00 AM Room1 [PL1] Plenary Talk 1 ○Christopher A. Schuh (Department of Materials Science and Engineering, MIT, USA) Plenary Talk | Plenary Talk [PL2] Plenary Talk 2 Chair: Alexey Lyulin(Technische Universiteit Eindhoven, The Netherlands) 11:00 AM - 11:50 AM Room1 [PL2] Plenary Talk 2 ○Maenghyo Cho (School of Mechanical and Aerospace Engineering, Seoul National University, Korea) ©The 9th International Conference on Multiscale Materials Modeling Mon. Oct 29, 2018 Symposium The 9th International Conference on Multiscale Materials Modeling Mon. Oct 29, 2018 Sauzay2, Mihai Cosmin Marinica1, Normand Mousseau3 Room1 (1.SRMP-CEA Saclay, France, 2.SRMA-CEA Saclay, France, 3.Département de Physique, Université de Symposium | C. Crystal Plasticity: From Electrons to Dislocation Montréal , Canada) Microstructure [SY-C1] Symposium C-1 Symposium | C. Crystal Plasticity: From Electrons to Dislocation Chair: Emmanuel Clouet(CEA Saclay, SRMP, France) Microstructure 1:30 PM - 3:15 PM Room1 [SY-C2] Symposium C-2 Chair: Stefan Sandfeld(Chair of Micromechanical Materials [SY-C1] Kinetic Monte Carlo model of screw dislocation- Modelling, TU Bergakademie Freiberg, Germany) solute coevolution in W-Re alloys 3:45 PM - 5:30 PM Room1 Yue Zhao1, Lucile Dezerald3, ○Jaime Marian1,2 (1.Dept. [SY-C2] Finite deformation Mesoscale Field Dislocation of Materials Science
  • Inhibition of Oxidation in Nuclear Graphite

    Inhibition of Oxidation in Nuclear Graphite

    NEA/NSC/WPFC/DOC(2015)9 Inhibition of oxidation in nuclear graphite Philip L. Winston, James W. Sterbentz and William E. Windes Idaho National Laboratory, United States Abstract Graphite is a fundamental material of high-temperature gas-cooled nuclear reactors, providing both structure and neutron moderation. Its high thermal conductivity, chemical inertness, thermal heat capacity, and high thermal structural stability under normal and off-normal conditions contribute to the inherent safety of these reactor designs. One of the primary safety issues for a high-temperature graphite reactor core is the possibility of rapid oxidation of the carbon structure during an off-normal design basis event where an oxidising atmosphere (air ingress) can be introduced to the hot core. Although the current Generation IV high-temperature reactor designs attempt to mitigate any damage caused by a postualed air ingress event, the use of graphite components that inhibit oxidation is a logical step to increase the safety of these reactors. Recent experimental studies of graphite containing between 5.5 and 7 wt% boron carbide (B4C) indicate that oxidation is dramatically reduced even at prolonged exposures at temperatures up to 900°C. The proposed addition of B4C to graphite components in the nuclear core would necessarily be enriched in B-11 isotope in order to minimise B-10 neutron absorption and graphite swelling. The enriched boron can be added to the graphite during billet fabrication. Experimental oxidation rate results and potential applications for borated graphite in nuclear reactor components will be discussed. Introduction Current Generation IV high-temperature gas-cooled reactors (HTR) are predominately constructed of graphite structural components and graphite fuel elements.
  • Management of Radioactive Waste Containing Graphite: Overview of Methods

    Management of Radioactive Waste Containing Graphite: Overview of Methods

    energies Review Management of Radioactive Waste Containing Graphite: Overview of Methods Leon Fuks * , Irena Herdzik-Koniecko, Katarzyna Kiegiel and Grazyna Zakrzewska-Koltuniewicz Centre for Radiochemistry and Nuclear Chemistry, Institute of Nuclear Chemistry and Technology, 16 Dorodna, 03-161 Warszawa, Poland; i.herdzik@ichtj.waw.pl (I.H.-K.); k.kiegiel@ichtj.waw.pl (K.K.); g.zakrzewska@ichtj.waw.pl (G.Z.-K.) * Correspondence: leon.ichtj@gmail.com; Tel.: +48-22-504-1360 Received: 30 July 2020; Accepted: 4 September 2020; Published: 7 September 2020 Abstract: Since the beginning of the nuclear industry, graphite has been widely used as a moderator and reflector of neutrons in nuclear power reactors. Some reactors are relatively old and have already been shut down. As a result, a large amount of irradiated graphite has been generated. Although several thousand papers in the International Nuclear Information Service (INIS) database have discussed the management of radioactive waste containing graphite, knowledge of this problem is not common. The aim of the paper is to present the current status of the methods used in different countries to manage graphite-containing radioactive waste. Attention has been paid to the methods of handling spent TRISO fuel after its discharge from high-temperature gas-cooled reactors (HTGR) reactors. Keywords: graphite; irradiated graphite; graphite processing; radioactive waste; waste management; waste disposal; spent TRISO fuel 1. Introduction As of December 31, 2018, 451 nuclear power reactors were in operation and produced 392,779 MWe of electricity. Fifty-five reactors, with a net capacity of 57,441 MWe, were under construction, while 172 reactors were permanently shut down [1].
  • Actinides Input to the Dose in the Irradiated Graphite of RBMK-1500 Reactor

    Actinides Input to the Dose in the Irradiated Graphite of RBMK-1500 Reactor

    Nuclear Engineering and Design 300 (2016) 530–535 Contents lists available at ScienceDirect Nuclear Engineering and Design jou rnal homepage: www.elsevier.com/locate/nucengdes Actinides input to the dose in the irradiated graphite of RBMK-1500 reactor a,∗ a a a a a R. Plukiene˙ , A. Plukis , A. Puzas , R. Gvozdaite˙ , V. Barkauskas , G. Duskesasˇ , b b a J.V. Cizdziel , D. Bussan , V. Remeikis a Institute of Physics, Center for Physical Sciences and Technology, Savanoriu˛ pr. 231, LT-02300 Vilnius, Lithuania b University of Mississippi, Department of Chemistry and Biochemistry, 305 Coulter Hall, University, Oxford, MS 38677, USA h i g h l i g h t s • Actinides input to the dose in RBMK-1500 reactor graphite was estimated. • SCALE 6.1 and MCNPX models were used to calculate actinides specific activities. • ORIGEN-ARP was used for gamma power, neutron source and effective dose calculation. • Concentrations of Pu, Am and Cm isotopes in the RBMK graphite sample were measured. • 244 Cm was found to be a critical contributor to effective dose of the personnel. a r t i c l e i n f o a b s t r a c t Article history: The purpose of this work is to indicate the actinides input to the total radiation dose caused by the Received 25 May 2015 irradiated graphite of the RBMK-1500 reactor in comparison to the dose delivered by other nuclides. Received in revised form 27 January 2016 We used computer codes (SCALE 6.1 and MCNPX 2.7) to estimate the dose rate delivered by actinides Accepted 4 February 2016 244 giving special attention to the Cm isotope as a critical contributor to the total activity of actinides in the spent graphite for approximately up to 200 years.
  • Investigation on Conversion of I-Graphite from Decommissioning of Chernobyl Npp Into a Stable Waste Form Acceptable for Long Term Storage and Disposal

    Investigation on Conversion of I-Graphite from Decommissioning of Chernobyl Npp Into a Stable Waste Form Acceptable for Long Term Storage and Disposal

    INVESTIGATION ON CONVERSION OF I-GRAPHITE FROM DECOMMISSIONING OF CHERNOBYL NPP INTO A STABLE WASTE FORM ACCEPTABLE FOR LONG TERM STORAGE AND DISPOSAL BORYS ZLOBENKO, YRIY FEDORENKO, VICTOR YATZENKO, BORYS SHABALIN, VADIM SKRIPKIN National Academy of Sciences of Ukraine: State Institution “Institute of Environmental Geochemistry” Department of Nuclear Geochemistry (Radiocarbon Laboratory), Kyiv, Ukraine INTRODUCTION For Ukraine, the main radiocarbon (14C) source is irradiated graphite from Chernobyl Nuclear Power Plant. The ChNPP is a decommissioned nuclear power station about 14 km northwest of the city of Chernobyl, and 110 km north of Kyiv. The ChNPP had four RBMK reactor units. The commissioning of the first reactor in 1977 was followed by reactor No. 2 (1978), No. 3 (1981), and No.4 (1983). Reactors No.3 and 4 were second generation units, whereas Nos.1 and 2 were first-generation units. RBMK is an acronym for "High Power Channel-type Reactor" of a class of graphite-moderated nuclear power reactor with individual fuel channels that uses ordinary water as its coolant and graphite as its moderator. The combination of graphite moderator and water coolant is found in no other type of nuclear reactor. Parameters RBMK-1000 Thermal power, MW 3840 Core diameter, m 11.80 Core height, m 7.0 Core volume, m 765 Mean specific power 5.02 per core volume, MW/m Mean specific power 20.8 per fuel quantity, MW/t Mean power per fuel 18.3 rod length, kW/m On September 9, 1982, a partial core meltdown occurred in Reactor No. 1 at the Chernobyl plant. The extent of the accident was not made public until several years later.
  • Nuclear Graphite - Fission Reactor Brief Outline of Experience and Understanding

    Nuclear Graphite - Fission Reactor Brief Outline of Experience and Understanding

    Nuclear Graphite - Fission Reactor Brief Outline of Experience and Understanding Professor Barry J Marsden and Dr. Graham N Hall Nuclear Graphite Research Group The University of Manchester 20 March 2013 School of Mechanical, Aerospace and Civil Engineering, University of Manchester, PO Box 88, Manchester, M13 9PL Tel: +44 (0) 161 275 4399, barry.marsden@manchester.ac.uk Overview • Nuclear Graphite – Use, Manufacture, Microstructure • Irradiation Damage to Crystal Structure • Radiolytic Oxidation • Physical Changes – to Polycrystalline Graphite due to Fast Neutron Damage and Radiolytic Oxidation • Irradiation Creep Use of Graphite in the Nuclear Industry • Moderator – Slow down neutrons by scattering – High scatter cross-section – Low absorption cross-section • Reflector – Reflects neutrons back into the core – Protect surrounding supports structure and pressure vessel • Major Structural Component – Provided channels for control rods and coolant gas • Neutron Shield – Boronated graphite • Thermal columns in research reactors • Moulds for casting uranium fuel Type of Graphite Moderated Reactors • Air-cooled – Chicago Pile, GLEEP, BEPO, Windscale Piles, G1-France • Light Water-cooled Graphite Moderated – Hanford, Russian-PPR, RBMK • Carbon Dioxide Cooled – UK and French Magnox reactors, AGR • Helium Cooled – Dragon, Peach Bottom, Fort St. Vrain, THTR, AVR – HTR, HTR-10 China, HTTR Japan, PBMR South Africa – Generation IV - VHTR Chicago Pile 1 Typical Graphite Components Torness Core – During Construction HTR-10 During Construction in China
  • Nuclear Engineering and Technology 52 (2020) 797E801

    Nuclear Engineering and Technology 52 (2020) 797E801

    Nuclear Engineering and Technology 52 (2020) 797e801 Contents lists available at ScienceDirect Nuclear Engineering and Technology journal homepage: www.elsevier.com/locate/net Original Article Proposal of a prototype plant based on the exfoliation process for the treatment of irradiated graphite * Silvia Pozzetto a, Mauro Capone a, Nadia Cherubini a, Maria Letizia Cozzella a, , Alessandro Dodaro a, Giambattista Guidi b a ENEA Italian National Agency for New Technologies, Energy and Sustainable Economic Development, Nuclear Material Characterization Laboratory and Nuclear Waste Management, Rome, Italy b ENEA - Italian National Agency for New Technologies, Energy and Sustainable Economic Development, Energy Technology Department and Guglielmo Marconi University, Rome, Italy article info abstract Article history: Most of irradiated graphite that should be disposed comes from moderators and reflectors of nuclear Received 18 March 2019 power plants. The quantity of irradiated graphite could be higher in the future if high-temperature re- Received in revised form actors (HTRs) will be deployed. In this case noteworthy quantities of fuel pebbles containing semi- 11 August 2019 graphitic carbonaceous material should be added to the already existing 250,000 tons of irradiated Accepted 16 September 2019 graphite. Industry graphite is largely used in industrial applications for its high thermal and electrical Available online 28 September 2019 conductivity and thermal and chemical resistance, making it a valuable material. Irradiated graphite constitutes a waste management challenge owing to the presence of long-lived radionuclides, such as 14C Keywords: 36 Irradiated graphite and Cl. 14C In the ENEA Nuclear Material Characterization Laboratory it has been successfully designed a pro- Prototype plant cedure based on the exfoliation process organic solvent assisted, with the purpose of investigate the Solvent recycling possibility of achieving graphite significantly less toxic that could be recycled for other purpose [1].
  • Nuclear Graphite Waste Management

    Nuclear Graphite Waste Management

    Technical Committee meeting held in Manchester, United Kingdom, o 18-20 October 1999 o ro 00 CD O Nuclear Graphite Waste Management Foreword Copyright/Editorial note Contents Summary List of participants Related IAEA priced publications INTERNATIONAL ATOMIC ENERGY AGENCY Copyright © IAEA, 2001 Published by the IAEA in Austria May 2001 Individual papers may be downloaded for personal use; single printed copies may be made for use in research and teaching. Redistribution or sale of any material on the CD-ROM in machine readable or any other form is prohibited. EDITORIAL NOTE This publication has been prepared from the original material as submitted by the authors. The views expressed do not necessarily reflect those of the IAEA, the governments of the nominating Member States or the nominating organizations. The use of particular designations of countries or territories does not imply any judgement by the publisher, the IAEA, as to the legal status of such countries or territories, of their authorities and institutions or of the delimitation of their boundaries. The mention of names of specific companies or products (whether or not indicated as registered) does not imply any intention to infringe proprietary rights, nor should it be construed as an endorsement or recommendation on the part of the IAEA. The authors are responsible for having obtained the necessary permission for the IAEA to reproduce, translate or use material from sources already protected by copyrights. FOREWORD Graphite and carbon have been used as a moderator and reflector of neutrons in more than one hundred nuclear power plants, mostly in the United Kingdom (Magnox and AGRs), France (UNGGs), the former USSR (RBMK), the United States of America (HTR) and Spain.
  • Nuclear Graphite Development, Operational Problems, and Resolution of These Problems at the Hanford Production Reactors'

    Nuclear Graphite Development, Operational Problems, and Resolution of These Problems at the Hanford Production Reactors'

    NUCLEAR GRAPHITE DEVELOPMENT, OPERATIONAL PROBLEMS, AND RESOLUTION OF THESE PROBLEMS AT THE HANFORD PRODUCTION REACTORS' W.C. MORGAN Pacific Northwest Laboratory, XA9642903 Richland, Washington, USA Abstract The first reactors designed for the whole-scale production of special nuclear materials were the graphite-moderated B, D, and F Reactors at the Hanford Engineering Works, northwest of Richland, WA (USA). These three Hanford Production Reactors (and the three generations of horizontally-tubed, water-cooled, graphite-moderated reactors that followed them) served as test beds for the development of improved nuclear-grade graphites. They also presented challenges to reactor operations staff and the scientific-support staff, as the effects of neutron radiation manifested itself through the changes in dimensions and physical properties of the graphite moderator bars. In-depth studies at other research establishments have greatly expanded current knowledge regarding radiation-induced changes in the chemical and physical properties of graphites, the effects of manufacturing variables (especially precursor materials) on the magnitude of the changes, and the importance of reactor design and operational variables that can minimize the impact of these changes on reactor operations. However, at the Hanford Production Reactors, knowledge regarding the effects of neutron radiation on graphite was gained by observation of the effects of those changes on the operational characteristics of the reactors, the physical distortions of the graphite moderator